General
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 15 GPa Show Supplier Material materials with Elastic modulus of 15 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | dry | ISO 527-1/-2 | |
Flexural modulus | 14 GPa Show Supplier Material materials with Flexural modulus of 14 GPa | dry | ISO 178 | |
Flexural yield strength | 255 MPa Show Supplier Material materials with Flexural yield strength of 255 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.8 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | 2 mm | IEC 60695-2-13 | ||
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | 3 mm | IEC 60695-2-13 | |||
Heat deflection temperature | 276 °C Show Supplier Material materials with Heat deflection temperature of 276 °C | dry | ISO 75-1/-2 | 2 MPa | ||
282 °C Show Supplier Material materials with Heat deflection temperature of 282 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 286 °C Show Supplier Material materials with Melting point of 286 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4.2 [-] Show Supplier Material materials with Dielectric constant of 4.2 [-] | dry | IEC 60250 | 1GHz |
4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | conditioned | IEC 60250 | 1GHz | |
Dielectric strength | 40 kV/mm Show Supplier Material materials with Dielectric strength of 40 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 100 [-] Show Supplier Material materials with Dissipation factor of 100 [-] | dry | IEC 60250 | 1GHz |
160 [-] Show Supplier Material materials with Dissipation factor of 160 [-] | conditioned | IEC 60250 | 1GHz |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | USB-C Connectors, DDR DIMM Connectors | |
Certifications | Yellow Card Available | |
Fillers | 45% Glass Fiber |