General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Coefficient of friction, kinetic | 0.8 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.8 [-] | dry | ISO 8295 |
Coefficient of friction, static | 1.4 [-] Show Supplier Material materials with Coefficient of friction, static of 1.4 [-] | dry | ISO 8295 |
Density | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Water absorption | 9 % Show Supplier Material materials with Water absorption of 9 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.47 GPa Show Supplier Material materials with Elastic modulus of 0.47 GPa | dry | DSM-Method, 50 mm/min | |
Elongation | 350 % Show Supplier Material materials with Elongation of 350 % | dry | ISO 527-3 | Parallel |
Tensile strength | 96 MPa Show Supplier Material materials with Tensile strength of 96 MPa | dry | ISO 527-3 | Parallel |
Yield strength | 34 MPa Show Supplier Material materials with Yield strength of 34 MPa | dry | ISO 527-3 | Parallel |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Specific heat capacity | 1550 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 1550 J/(kg·K) | dry | - | |
2250 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 2250 J/(kg·K) | dry |
Optical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Transparency | 85 | dry | DSM method |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt viscosity | 260 °C | 810 Pa·s Show Supplier Material materials with Melt viscosity of 810 Pa·s | dry | DSM method, 260 °C |
Viscosity number | 195 cm³/gr Show Supplier Material materials with Viscosity number of 195 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|