General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.39 g/cm³ Show Supplier Material materials with Density of 1.39 g/cm³ | dry | ISO 1183 | |
Limiting oxygen index | 29.0 % Show Supplier Material materials with Limiting oxygen index of 29.0 % | dry | ISO 4589-1/-2 | |
Moisture absorption | 2.35 % Show Supplier Material materials with Moisture absorption of 2.35 % | dry | Sim. to ISO 62 | |
Water absorption | 2.4 % Show Supplier Material materials with Water absorption of 2.4 % | dry | ISO 62 | at 23°C after 24h |
8.5 % Show Supplier Material materials with Water absorption of 8.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.4 GPa Show Supplier Material materials with Elastic modulus of 3.4 GPa | dry | ISO 527-1/-2 | |
Elongation | 20 % Show Supplier Material materials with Elongation of 20 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | dry | ISO 178 | |
Flexural yield strength | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | UL746B | 0.75 mm |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1140 g/cm³ Show Supplier Material materials with Density of melt of 1140 g/cm³ | dry | - | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal | |
Thermal conductivity of melt | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K) | dry | - |