General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 | |
Water absorption | 1.8 % Show Supplier Material materials with Water absorption of 1.8 % | dry | ISO 62 | at 23°C after 24h |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.02 GPa Show Supplier Material materials with Elastic modulus of 0.02 GPa | dry | ISO 527-1/-2 | |
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | |
980 % Show Supplier Material materials with Elongation of 980 % | dry | ISO 527-1/-2 | ||
Hardness, Shore A | 79 [-] Show Supplier Material materials with Hardness, Shore A of 79 [-] | dry | ISO 868 | 15s |
80 [-] Show Supplier Material materials with Hardness, Shore A of 80 [-] | dry | ISO 868 | 3s | |
Hardness, Shore D | 18 [-] Show Supplier Material materials with Hardness, Shore D of 18 [-] | dry | ISO 868 | 15s |
19 [-] Show Supplier Material materials with Hardness, Shore D of 19 [-] | dry | ISO 868 | 3s | |
Tensile strength | 14.4 MPa Show Supplier Material materials with Tensile strength of 14.4 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Glass transition temperature | -68 °C Show Supplier Material materials with Glass transition temperature of -68 °C | dry | ASTM D5026/D7028 | DMTA (tan d) | |
Melting point | 165 °C Show Supplier Material materials with Melting point of 165 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 1 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 1 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 1 mm |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 76 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 76 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.7 % Show Supplier Material materials with Shrinkage of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Shrinkage of 1 % | dry | Sim. to ISO 294-4 | Normal | ||
Viscosity number | 3.32 cm³/gr Show Supplier Material materials with Viscosity number of 3.32 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Smartwatch Straps | |
Certifications | Yellow Card Available |