General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 1.3 GPa Show Supplier Material materials with Elastic modulus of 1.3 GPa | conditioned | ISO 527-1/-2 | |
3.1 GPa Show Supplier Material materials with Elastic modulus of 3.1 GPa | dry | ISO 527-1/-2 | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | |
Flexural modulus | 1.1 GPa Show Supplier Material materials with Flexural modulus of 1.1 GPa | conditioned | ISO 178 | |
2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | dry | ISO 178 | ||
Flexural yield strength | 54 MPa Show Supplier Material materials with Flexural yield strength of 54 MPa | conditioned | ISO 178 | |
110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | dry | ISO 179/1eA |
23 °C | 26 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 26 kJ/m² | conditioned | ISO 179/1eA |
Thermal
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Flammability | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Heat deflection temperature | 75 °C Show Supplier Material materials with Heat deflection temperature of 75 °C | dry | ISO 75-1/-2 | 2 MPa | ||
169 °C Show Supplier Material materials with Heat deflection temperature of 169 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.81 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.81 mm | UL746B | ||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | dry | 0.81 mm | UL746B |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 100Hz |
4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
Dielectric strength | 26 kV/mm Show Supplier Material materials with Dielectric strength of 26 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 110 [-] Show Supplier Material materials with Dissipation factor of 110 [-] | dry | IEC 62631-2-1 | 100Hz |
220 [-] Show Supplier Material materials with Dissipation factor of 220 [-] | dry | IEC 62631-2-1 | 1MHz | |
Surface resistivity | 2e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 230 °C | 34 g/10min Show Supplier Material materials with Melt mass-flow rate of 34 g/10min | dry | ISO 1133 | |
Melt volume-flow rate | 230 °C | 34 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 34 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | Sim. to ISO 294-4 | Normal | ||
Viscosity number | 138 cm³/gr Show Supplier Material materials with Viscosity number of 138 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |