General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Water absorption | 5.2 % Show Supplier Material materials with Water absorption of 5.2 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7 GPa Show Supplier Material materials with Elastic modulus of 7 GPa | dry, conditioned | ISO 527-1/-2 | |
Elongation | 2 % Show Supplier Material materials with Elongation of 2 % | dry | ISO 527-1/-2 | |
2.1 % Show Supplier Material materials with Elongation of 2.1 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 7 GPa Show Supplier Material materials with Flexural modulus of 7 GPa | dry, conditioned | ISO 178 | |
Flexural yield strength | 175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | conditioned | ISO 178 | |
180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry, conditioned | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | dry, conditioned | ISO 179/1eU |
Tensile strength | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | dry | ISO 527-1/-2 | |
110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | conditioned | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 300 °C Show Supplier Material materials with Ball pressure temperature of 300 °C | dry | IEC 60695-10-2 | |||
Coefficient of thermal expansion | 4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ASTM D696 | Parallel | ||
5.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.5e-07 1/K | dry | ASTM D696 | Normal | |||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | 125 °C Show Supplier Material materials with Glass transition temperature of 125 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.35 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | |||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | dry | IEC 60695-2-13 | 0.75 mm | ||
775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | dry | IEC 60695-2-13 | 0.35 mm | |||
Heat deflection temperature | 300 °C Show Supplier Material materials with Heat deflection temperature of 300 °C | dry | ISO 75-1/-2 | 2 MPa | ||
320 °C Show Supplier Material materials with Heat deflection temperature of 320 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 325 °C Show Supplier Material materials with Melting point of 325 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |