General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.41 g/cm³ Show Supplier Material materials with Density of 1.41 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Water absorption | 5.7 % Show Supplier Material materials with Water absorption of 5.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7.3 GPa Show Supplier Material materials with Elastic modulus of 7.3 GPa | conditioned | ISO 527-1/-2 | |
11.5 GPa Show Supplier Material materials with Elastic modulus of 11.5 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongation of 7 % | conditioned | ISO 527-1/-2 | ||
Impact strength, Charpy notched | -30 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | dry | ISO 179/1eA | |
23 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 30 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU |
-30 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | conditioned | ISO 527-1/-2 | |
175 MPa Show Supplier Material materials with Tensile strength of 175 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | conditioned | IEC 60112 | |
Dielectric constant | 3.3 [-] Show Supplier Material materials with Dielectric constant of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 90 [-] Show Supplier Material materials with Dissipation factor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Dissipation factor of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 75 g/10min Show Supplier Material materials with Melt mass-flow rate of 75 g/10min | dry | ISO 1133 | ||
Melt volume-flow rate | 275 °C | 60 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 60 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.36 % Show Supplier Material materials with Shrinkage of 0.36 % | dry | ISO 294-4 | Parallel | |
0.89 % Show Supplier Material materials with Shrinkage of 0.89 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag Containers | |
Fillers | 40% Glass Fiber |