General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | dry | ISO 1183 |
Limiting oxygen index | 24 % Show Supplier Material materials with Limiting oxygen index of 24 % | dry | ISO 4589-1/-2 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Water absorption | 5.8 % Show Supplier Material materials with Water absorption of 5.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | dry | ISO 527-1/-2 | |
Elongation | 20 % Show Supplier Material materials with Elongation of 20 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 3.6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3.6 kJ/m² | dry | ISO 179/1eA |
23 °C | 5.4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.4 kJ/m² | dry | ISO 179/1eA | |
Tensile strength | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt mass-flow rate | 280 °C | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | dry | ISO 1133 |
Melt volume-flow rate | 280 °C | 26 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 26 cm³/10min | dry | ISO 1133 |
Viscosity number | 170 cm³/gr Show Supplier Material materials with Viscosity number of 170 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |