General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | dry | ISO 527-1/-2 | |
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 2 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 24 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 60 °C Show Supplier Material materials with Heat deflection temperature of 60 °C | dry | ISO 75-1/-2 | 2 MPa | |
145 °C Show Supplier Material materials with Heat deflection temperature of 145 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property |
---|