General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.07 g/cm³ Show Supplier Material materials with Density of 1.07 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Water absorption | 7 % Show Supplier Material materials with Water absorption of 7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 1.8 GPa Show Supplier Material materials with Elastic modulus of 1.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Flexural modulus | 1.6 GPa Show Supplier Material materials with Flexural modulus of 1.6 GPa | dry | ISO 178 | |
Flexural yield strength | 65 MPa Show Supplier Material materials with Flexural yield strength of 65 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | dry | ISO 179/1eA |
-30 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 65 kJ/m² | dry | ISO 179/1eA | |
23 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 75 kJ/m² | conditioned | ISO 179/1eA | |
Puncture energy | -40 °C | 8 J Show Supplier Material materials with Puncture energy of 8 J | dry | ISO 6603-2 |
23 °C | 50 J Show Supplier Material materials with Puncture energy of 50 J | dry | ISO 6603-2 | |
Puncture force | -40 °C | 2900 N Show Supplier Material materials with Puncture force of 2900 N | dry | ISO 6603-2 |
23 °C | 3600 N Show Supplier Material materials with Puncture force of 3600 N | dry | ISO 6603-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 50 °C Show Supplier Material materials with Heat deflection temperature of 50 °C | dry | ISO 75-1/-2 | 2 MPa | |
130 °C Show Supplier Material materials with Heat deflection temperature of 130 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Thermal diffusivity | 9.37e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 9.37e-08 mm²/s | dry | - |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 869 g/cm³ Show Supplier Material materials with Density of melt of 869 g/cm³ | dry | - |
Melt mass-flow rate | 16 g/10min Show Supplier Material materials with Melt mass-flow rate of 16 g/10min | dry | ISO 1133 |
Specific heat capacity melt | 2740 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2740 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.22 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.22 W/(m·K) | dry | - |
Technological properties