Arnitel® EL740-08

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Arnitel® is a high-performance ThermoPlastic Copolyester (TPC) that offers you a unique combination of flexibility, high temperature resistance and strength - plus excellent processing characteristics.
In industries ranging from automotive to E&E, Arnitel® is increasingly being as a lighter, smarter, greener alternative to conventional rubbers – reducing environmental impact and ultimately, system costs.
The product is supported by an experienced and knowledgeable global team continuously working on new ideas and applications, as well as exploring new markets. By listening to your needs and understanding your process and products, we develop solutions that make a real difference.

Datasheet URL:

Arnitel® EL740-08

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

0.83 g/cm³

Show Supplier Material materials with Density of 0.83 g/cm³

dry

ISO 60

1.29 g/cm³

Show Supplier Material materials with Density of 1.29 g/cm³

dry

ISO 1183

Moisture absorption

0.15 %

Show Supplier Material materials with Moisture absorption of 0.15 %

dry

Sim. to ISO 62

Water absorption

0.6 %

Show Supplier Material materials with Water absorption of 0.6 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.8 GPa

Show Supplier Material materials with Elastic modulus of 0.8 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

250 %

Show Supplier Material materials with Elongation of 250 %

dry

ISO 527-1/-2

Elongation at yield

17 %

Show Supplier Material materials with Elongation at yield of 17 %

dry

ISO 527-1/-2

Hardness, Shore D

70 [-]

Show Supplier Material materials with Hardness, Shore D of 70 [-]

dry

ISO 868

3s

Impact strength, Charpy notched

-30 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

dry

ISO 179/1eA

23 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

dry

ISO 179/1eA

Tear strength

215 kN/m

Show Supplier Material materials with Tear strength of 215 kN/m

dry

ISO 34-1; Method B

Tensile strength

43 MPa

Show Supplier Material materials with Tensile strength of 43 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardThicknessPressureComment

Coefficient of thermal expansion

1.65e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.65e-06 1/K

dry

ISO 11359-1/-2

Parallel

1.65e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.65e-06 1/K

dry

ISO 11359-1/-2

Normal

Flammability

HB

dry

IEC 60695-11-10

1.5 mm

UL recognition :Yes

Heat deflection temperature

120 °C

Show Supplier Material materials with Heat deflection temperature of 120 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

221 °C

Show Supplier Material materials with Melting point of 221 °C

dry

ISO 11357-1/-3

10°C/min

Relative temperature index, electrical

50 °C

Show Supplier Material materials with Relative temperature index, electrical of 50 °C

dry

UL746B

2 mm

Relative temperature index, mechanical impact

50 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C

dry

UL746B

2 mm

Relative temperature index, mechanical strength

50 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C

dry

UL746B

2 mm

Thermal diffusivity

5.54e-08 mm²/s

Show Supplier Material materials with Thermal diffusivity of 5.54e-08 mm²/s

dry

-

Vicat softening temperature

160 °C

Show Supplier Material materials with Vicat softening temperature of 160 °C

dry

ISO 306

50°C/h 50N

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

dry

IEC 60112

Dielectric constant

3.3 [-]

Show Supplier Material materials with Dielectric constant of 3.3 [-]

dry

IEC 62631-2-1

1MHz

3.7 [-]

Show Supplier Material materials with Dielectric constant of 3.7 [-]

dry

IEC 62631-2-1

100Hz

Dielectric strength

23 kV/mm

Show Supplier Material materials with Dielectric strength of 23 kV/mm

dry

IEC 60243-1

Dissipation factor

300 [-]

Show Supplier Material materials with Dissipation factor of 300 [-]

dry

IEC 62631-2-1

1MHz

Volume resistivity

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Density of melt

950 g/cm³

Show Supplier Material materials with Density of melt of 950 g/cm³

dry

-

Melt volume-flow rate

230 °C

18 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min

dry

ISO 1133

Shrinkage

1.75 %

Show Supplier Material materials with Shrinkage of 1.75 %

dry

Sim. to ISO 294-4

Parallel

2 %

Show Supplier Material materials with Shrinkage of 2 %

dry

Sim. to ISO 294-4

Normal

Specific heat capacity melt

1900 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K)

dry

-

Thermal conductivity of melt

0.1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K)

dry

-

Technological properties

Property
Certifications

Yellow Card Available