Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.3 g/cm³ Show Supplier Material materials with Density of 1.3 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 6.4 GPa Show Supplier Material materials with Elastic modulus of 6.4 GPa | dry | ISO 527-1/-2 |
4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | conditioned | ISO 527-1/-2 | ||
6.8 GPa Show Supplier Material materials with Elastic modulus of 6.8 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | dry | ISO 527-1/-2 | |
150 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 3.6 % Show Supplier Material materials with Elongation of 3.6 % | dry | ISO 527-1/-2 |
3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 | ||
5.3 % Show Supplier Material materials with Elongation of 5.3 % | conditioned | ISO 527-1/-2 | ||
120 °C | 8.5 % Show Supplier Material materials with Elongation of 8.5 % | dry | ISO 527-1/-2 | |
150 °C | 9.5 % Show Supplier Material materials with Elongation of 9.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 42 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 42 kJ/m² | dry | ISO 179/1eA |
23 °C | 5.8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.8 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 5.7 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 5.7 kJ/m² | dry | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | -40 °C | 140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | dry | ISO 527-1/-2 |
70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | conditioned | ISO 527-1/-2 | ||
110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 | ||
120 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | dry | ISO 527-1/-2 | |
150 °C | 46 MPa Show Supplier Material materials with Tensile strength of 46 MPa | dry | ISO 527-1/-2 |
Thermal
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |