General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.03 GPa Show Supplier Material materials with Elastic modulus of 0.03 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | ||
Hardness, Shore A | 85 [-] Show Supplier Material materials with Hardness, Shore A of 85 [-] | dry | ISO 868 | 3s |
Hardness, Shore D | 35 [-] Show Supplier Material materials with Hardness, Shore D of 35 [-] | dry | ISO 868 | 3s |
Tensile strength | 15 MPa Show Supplier Material materials with Tensile strength of 15 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 158 °C Show Supplier Material materials with Melting point of 158 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 32 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 32 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Midsole athletic shoes |