General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.39 g/cm³ Show Supplier Material materials with Density of 1.39 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | dry | ISO 527-1/-2 | |
Flexural modulus | 8.7 GPa Show Supplier Material materials with Flexural modulus of 8.7 GPa | dry | ISO 178 | |
Flexural yield strength | 225 MPa Show Supplier Material materials with Flexural yield strength of 225 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Ball pressure temperature | 255 °C Show Supplier Material materials with Ball pressure temperature of 255 °C | dry | IEC 60695-10-2 | ||
Glass transition temperature | 60 °C Show Supplier Material materials with Glass transition temperature of 60 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | |
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | ||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | - | dry | Sim. to IEC 60112 | Above 600V |
600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | ||
Dielectric strength | 40 kV/mm Show Supplier Material materials with Dielectric strength of 40 kV/mm | dry | IEC 60243-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | EV Charging Plugs | |
Certifications | Yellow Card Available | |
Fillers | 25% Glass Fiber |