General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.7 % Show Supplier Material materials with Moisture absorption of 2.7 % | dry | Sim. to ISO 62 |
Water absorption | 7.3 % Show Supplier Material materials with Water absorption of 7.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 0.5 GPa Show Supplier Material materials with Elastic modulus of 0.5 GPa | conditioned | ISO 527-1/-2 | |
1.9 GPa Show Supplier Material materials with Elastic modulus of 1.9 GPa | dry | ISO 527-1/-2 | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry, conditioned | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Flexural modulus | 1.8 GPa Show Supplier Material materials with Flexural modulus of 1.8 GPa | dry | ISO 178 | |
Flexural yield strength | 71 MPa Show Supplier Material materials with Flexural yield strength of 71 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m² | dry | ISO 179/1eA | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 100 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Vicat softening temperature | 130 °C Show Supplier Material materials with Vicat softening temperature of 130 °C | dry | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 275 °C | 35 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 35 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | High pressure type IV composite fuel tanks |