Akulon® K122/F

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K122/F

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

dry

Sim. to ISO 62

Water absorption

9.5 %

Show Supplier Material materials with Water absorption of 9.5 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

2.7 GPa

Show Supplier Material materials with Elastic modulus of 2.7 GPa

dry

ISO 527-1/-2

Elongation at yield

4.2 %

Show Supplier Material materials with Elongation at yield of 4.2 %

dry

ISO 527-1/-2

Impact strength, Charpy notched

23 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

dry

ISO 179/1eA

Thermal

PropertyValueConditionTesting StandardComment

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Thermal diffusivity

8.82e-08 mm²/s

Show Supplier Material materials with Thermal diffusivity of 8.82e-08 mm²/s

dry

-

Rheological Properties

PropertyValueConditionTesting Standard

Density of melt

960 g/cm³

Show Supplier Material materials with Density of melt of 960 g/cm³

dry

-

Specific heat capacity melt

2680 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2680 J/(kg·K)

dry

-

Thermal conductivity of melt

0.23 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.23 W/(m·K)

dry

-

Viscosity number

132 cm³/gr

Show Supplier Material materials with Viscosity number of 132 cm³/gr

dry

ISO 307, 1157, 1628