General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.24 g/cm³ Show Supplier Material materials with Density of 1.24 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Water absorption | 0.63 % Show Supplier Material materials with Water absorption of 0.63 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 0.31 GPa Show Supplier Material materials with Elastic modulus of 0.31 GPa | dry | ISO 527-1/-2 | ||
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
750 % Show Supplier Material materials with Elongation of 750 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 29.0 % Show Supplier Material materials with Elongation at yield of 29.0 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.3 GPa Show Supplier Material materials with Flexural modulus of 0.3 GPa | dry | ISO 178 | ||
Hardness, Shore D | 59 [-] Show Supplier Material materials with Hardness, Shore D of 59 [-] | dry | ISO 868 | 3s | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
Tear strength | 156 kN/m Show Supplier Material materials with Tear strength of 156 kN/m | dry | ISO 34-1; Method B | ||
168 kN/m Show Supplier Material materials with Tear strength of 168 kN/m | dry | ISO 34-1; Method B | |||
Tensile strength | 35 MPa Show Supplier Material materials with Tensile strength of 35 MPa | dry | ISO 527-1/-2 | ||
52 MPa Show Supplier Material materials with Tensile strength of 52 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Melting point | 212 °C Show Supplier Material materials with Melting point of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat softening temperature | 125 °C Show Supplier Material materials with Vicat softening temperature of 125 °C | dry | ISO 306 | 50°C/h 50N |
200 °C Show Supplier Material materials with Vicat softening temperature of 200 °C | dry | ISO 306 | 50°C/h 10N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4.1 [-] Show Supplier Material materials with Dielectric constant of 4.1 [-] | dry | IEC 62631-2-1 | 1MHz |
Dielectric strength | 22 kV/mm Show Supplier Material materials with Dielectric strength of 22 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 170 [-] Show Supplier Material materials with Dissipation factor of 170 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1.2e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.2e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 3.7 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 3.7 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Brake Tubing with Arnitel® CM622, Hydraulic Hoses |