General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt mass-flow rate | 230 °C | 34 g/10min Show Supplier Material materials with Melt mass-flow rate of 34 g/10min | dry | ISO 1133 |
Melt volume-flow rate | 230 °C | 30 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 30 cm³/10min | dry | ISO 1133 |
Viscosity number | 138 cm³/gr Show Supplier Material materials with Viscosity number of 138 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |