General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 3 % Show Supplier Material materials with Moisture absorption of 3 % | dry | Sim. to ISO 62 |
Water absorption | 10 % Show Supplier Material materials with Water absorption of 10 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.3 GPa Show Supplier Material materials with Elastic modulus of 3.3 GPa | dry | ISO 527-1/-2 | |
Elongation | 25 % Show Supplier Material materials with Elongation of 25 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.4e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.4e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 60 °C Show Supplier Material materials with Heat deflection temperature of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
160 °C Show Supplier Material materials with Heat deflection temperature of 160 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 2 mm | ||
Thermal diffusivity | 8.82e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 8.82e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry, conditioned | IEC 60112 | |
Dielectric constant | 3.4 [-] Show Supplier Material materials with Dielectric constant of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.9 [-] Show Supplier Material materials with Dielectric constant of 3.9 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | conditioned | IEC 60243-1 | |
27 kV/mm Show Supplier Material materials with Dielectric strength of 27 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 110 [-] Show Supplier Material materials with Dissipation factor of 110 [-] | dry | IEC 62631-2-1 | 100Hz |
220 [-] Show Supplier Material materials with Dissipation factor of 220 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Dissipation factor of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 960 g/cm³ Show Supplier Material materials with Density of melt of 960 g/cm³ | dry | - |
Specific heat capacity melt | 2680 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2680 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.23 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.23 W/(m·K) | dry | - |
Viscosity number | 214 cm³/gr Show Supplier Material materials with Viscosity number of 214 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |