Novamid® 1013GH15 1 NA/BK37

Alternative and trade names
PA6-GF15
Want to keep this datasheet? Save it now in your required format

Description

Novamid® is a high-quality polyamide, that has been developed as a special product line in order to cope with high demand levels from our Japanese customers.
Novamid® has seen various applications in various fields and various regions. From car to packaging, Novamid® is supported by an experienced and wide range of experts.

Datasheet URL:

Novamid® 1013GH15 1 NA/BK37

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.23 g/cm³

Show Supplier Material materials with Density of 1.23 g/cm³

dry

ISO 1183

Moisture absorption

2.4 %

Show Supplier Material materials with Moisture absorption of 2.4 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

3.3 GPa

Show Supplier Material materials with Elastic modulus of 3.3 GPa

conditioned

ISO 527-1/-2

5.8 GPa

Show Supplier Material materials with Elastic modulus of 5.8 GPa

dry

ISO 527-1/-2

Elongation

2.7 %

Show Supplier Material materials with Elongation of 2.7 %

dry

ISO 527-1/-2

8.7 %

Show Supplier Material materials with Elongation of 8.7 %

conditioned

ISO 527-1/-2

Flexural modulus

3 GPa

Show Supplier Material materials with Flexural modulus of 3 GPa

conditioned

ISO 178

5.4 GPa

Show Supplier Material materials with Flexural modulus of 5.4 GPa

dry

ISO 178

Flexural yield strength

120 MPa

Show Supplier Material materials with Flexural yield strength of 120 MPa

conditioned

ISO 178

200 MPa

Show Supplier Material materials with Flexural yield strength of 200 MPa

dry

ISO 178

Impact strength, Charpy notched

23 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

dry

ISO 179/1eA

23 °C

14.0 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m²

conditioned

ISO 179/1eA

Impact strength, Charpy unnotched

23 °C

39 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 39 kJ/m²

dry

ISO 179/1eU

23 °C

105 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 105 kJ/m²

conditioned

ISO 179/1eU

Tensile strength

75 MPa

Show Supplier Material materials with Tensile strength of 75 MPa

conditioned

ISO 527-1/-2

130 MPa

Show Supplier Material materials with Tensile strength of 130 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Heat deflection temperature

194 °C

Show Supplier Material materials with Heat deflection temperature of 194 °C

dry

ISO 75-1/-2

2 MPa

216 °C

Show Supplier Material materials with Heat deflection temperature of 216 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

400 V

Show Supplier Material materials with Comparative tracking index of 400 V

dry

IEC 60112

Dielectric constant

4 [-]

Show Supplier Material materials with Dielectric constant of 4 [-]

dry

IEC 62631-2-1

100Hz

4 [-]

Show Supplier Material materials with Dielectric constant of 4 [-]

dry

IEC 62631-2-1

1MHz

Dielectric strength

27 kV/mm

Show Supplier Material materials with Dielectric strength of 27 kV/mm

dry

IEC 60243-1

Dissipation factor

130 [-]

Show Supplier Material materials with Dissipation factor of 130 [-]

dry

IEC 62631-2-1

100Hz

230 [-]

Show Supplier Material materials with Dissipation factor of 230 [-]

dry

IEC 62631-2-1

1MHz

Surface resistivity

8e+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 8e+13 Ω/sq

conditioned

IEC 62631-3-2

Volume resistivity

6e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 6e+12 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Melt mass-flow rate

250 °C

18 g/10min

Show Supplier Material materials with Melt mass-flow rate of 18 g/10min

dry

ISO 1133

Melt volume-flow rate

250 °C

18 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min

dry

ISO 1133

Shrinkage

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

dry

ISO 294-4

Parallel

1.3 %

Show Supplier Material materials with Shrinkage of 1.3 %

dry

ISO 294-4

Normal

Technological properties

Property
Fillers

15% Glass Fiber