General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.15 g/cm³ Show Supplier Material materials with Density of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Water absorption | 0.7 % Show Supplier Material materials with Water absorption of 0.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.07 GPa Show Supplier Material materials with Elastic modulus of 0.07 GPa | dry | ISO 527-1/-2 | |
Elongation | 210 % Show Supplier Material materials with Elongation of 210 % | dry | ISO 527-1/-2 | |
740 % Show Supplier Material materials with Elongation of 740 % | dry | ISO 527-1/-2 | ||
Hardness, Shore D | 38 [-] Show Supplier Material materials with Hardness, Shore D of 38 [-] | dry | ISO 868 | 3s |
Tear strength | 88 kN/m Show Supplier Material materials with Tear strength of 88 kN/m | dry | ISO 34-1; Method B | |
103 kN/m Show Supplier Material materials with Tear strength of 103 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 17 MPa Show Supplier Material materials with Tensile strength of 17 MPa | dry | ISO 527-1/-2 | |
23 MPa Show Supplier Material materials with Tensile strength of 23 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 203 °C Show Supplier Material materials with Melting point of 203 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 10.5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 10.5 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Shrinkage of 2 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Boots and Bellows |