General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.12 g/cm³ Show Supplier Material materials with Density of 1.12 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 | |
13 % Show Supplier Material materials with Elongation of 13 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 4.3 % Show Supplier Material materials with Elongation at yield of 4.3 % | dry | ISO 527-1/-2 | |
Flexural modulus | 0.98 GPa Show Supplier Material materials with Flexural modulus of 0.98 GPa | conditioned | ISO 178 | |
2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | dry | ISO 178 | ||
Flexural yield strength | 48 MPa Show Supplier Material materials with Flexural yield strength of 48 MPa | conditioned | ISO 178 | |
95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 280 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 280 kJ/m² | dry, conditioned | ISO 179/1eU |
Tensile strength | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | dry | ISO 527-1/-2 |
Technological properties
Property |
---|