Xytron™ M5710T

Want to keep this datasheet? Save it now in your required format

Description

Xytron™ is a high performance plastic compound of DSM Engineering Plastics, which is based on PPS (polyphenylene sulphide).
Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.
Because of its outstanding properties, Xytron™ contributes to an excellent performance in many different applications.

Datasheet URL:

Xytron™ M5710T

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.86 g/cm³

Show Supplier Material materials with Density of 1.86 g/cm³

ISO 1183

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ISO 62, water at 23°C after 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

19 GPa

Show Supplier Material materials with Elastic modulus of 19 GPa

ISO 527-1/-2

Elongation

-40.0 °C

1.3 %

Show Supplier Material materials with Elongation of 1.3 %

ISO 527-1/-2

23.0 °C

1.3 %

Show Supplier Material materials with Elongation of 1.3 %

ISO 527-1/-2

120.0 °C

2.2 %

Show Supplier Material materials with Elongation of 2.2 %

ISO 527-1/-2

160.0 °C

2.3 %

Show Supplier Material materials with Elongation of 2.3 %

ISO 527-1/-2

Flexural modulus

23.0 °C

18 GPa

Show Supplier Material materials with Flexural modulus of 18 GPa

ISO 178

120.0 °C

10 GPa

Show Supplier Material materials with Flexural modulus of 10 GPa

ISO 178

160.0 °C

8 GPa

Show Supplier Material materials with Flexural modulus of 8 GPa

ISO 178

Unlock all property charts

Flexural yield strength

23.0 °C

280 MPa

Show Supplier Material materials with Flexural yield strength of 280 MPa

ISO 178

120.0 °C

160 MPa

Show Supplier Material materials with Flexural yield strength of 160 MPa

ISO 178

160.0 °C

120 MPa

Show Supplier Material materials with Flexural yield strength of 120 MPa

ISO 178

Unlock all property charts

Impact strength, Charpy notched

-30.0 °C

9.8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9.8 kJ/m²

ISO 179/1eA

23.0 °C

8.8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 8.8 kJ/m²

ISO 179/1eA

Unlock all property charts

Impact strength, Charpy unnotched

-30.0 °C

40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

ISO 179/1eU

23.0 °C

39 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 39 kJ/m²

ISO 179/1eU

Unlock all property charts

Tensile strength

-40.0 °C

220 MPa

Show Supplier Material materials with Tensile strength of 220 MPa

ISO 527-1/-2

23.0 °C

170 MPa

Show Supplier Material materials with Tensile strength of 170 MPa

ISO 527-1/-2

120.0 °C

105 MPa

Show Supplier Material materials with Tensile strength of 105 MPa

ISO 527-1/-2

160.0 °C

75 MPa

Show Supplier Material materials with Tensile strength of 75 MPa

ISO 527-1/-2

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-7 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-7 1/K

ISO 11359-1/-2, Parallel

Coefficient of thermal expansion, transverse

23.0 °C

3.5E-7 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.5E-7 1/K

ISO 11359-1/-2, Normal

Glass transition temperature

90 °C

Show Supplier Material materials with Glass transition temperature of 90 °C

ISO 11357-1/-2, (10°C/min)

Heat deflection temperature, 1.80 MPa

265 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 265 °C

ISO 75-1/-2

Melting point

280 °C

Show Supplier Material materials with Melting point of 280 °C

ISO 11357-1/-3, (10°C/min)

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

175 V

Show Supplier Material materials with Comparative tracking index of 175 V

IEC 60112

Dielectric constant

23.0 °C

4.5 [-]

Show Supplier Material materials with Dielectric constant of 4.5 [-]

IEC 60250, 5GHz

Dielectric strength

23.0 °C

26 kV/mm

Show Supplier Material materials with Dielectric strength of 26 kV/mm

IEC 60234

Dissipation factor, 5GHz

23.0 °C

50 [-]

Show Supplier Material materials with Dissipation factor, 5GHz of 50 [-]

IEC 60250, 5 GHz

Surface resistivity

23.0 °C

1.00E+15 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq

IEC 62631-3-2

Volume resistivity

23.0 °C

1.00E+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+13 Ω·cm

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

ISO 294-4, Parallel

Shrinkage, transverse

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage, transverse of 0.4 %

ISO 294-4, Normal

Technological properties

Property
Application areas

Crankshaft Covers, Rectifier, Water pump part