Description

Novamid® is a high-quality polyamide, that has been developed as a special product line in order to cope with high demand levels from our Japanese customers.
Novamid® has seen various applications in various fields and various regions. From car to packaging, Novamid® is supported by an experienced and wide range of experts.

Datasheet URL:

Novamid® AM1030 FR (F)

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

3.5 GPa

Show Supplier Material materials with Elastic modulus of 3.5 GPa

dry

ISO 527-1/-2

Elongation

7 %

Show Supplier Material materials with Elongation of 7 %

dry

ISO 527-1/-2

Elongation at yield

2.8 %

Show Supplier Material materials with Elongation at yield of 2.8 %

dry

ISO 527-1/-2

Impact strength, Charpy notched

23 °C

3 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

23 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m²

dry

ISO 179/1eU

Tensile strength

50 MPa

Show Supplier Material materials with Tensile strength of 50 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionThicknessTesting StandardComment

Flammability

V-0

dry

1.6 mm

IEC 60695-11-10

UL recognition :Yes

Glass transition temperature

58.0 °C

Show Supplier Material materials with Glass transition temperature of 58.0 °C

dry

ISO 11357-1/-2

10°C/min

Melting point

200 °C

Show Supplier Material materials with Melting point of 200 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties