Novamid® 2030 FC

Want to keep this datasheet? Save it now in your required format

Description

Novamid® is a high-quality polyamide, that has been developed as a special product line in order to cope with high demand levels from our Japanese customers.
Novamid® has seen various applications in various fields and various regions. From car to packaging, Novamid® is supported by an experienced and wide range of experts.

Datasheet URL:

Novamid® 2030 FC

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.8000000000000003 %

Show Supplier Material materials with Moisture absorption of 2.8000000000000003 %

dry

Sim. to ISO 62

Viscosity number

246 cm³/gr

Show Supplier Material materials with Viscosity number of 246 cm³/gr

dry

ISO 307, 1157, 1628

Thermal

PropertyValueConditionTesting StandardComment

Melting point

200 °C

Show Supplier Material materials with Melting point of 200 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt mass-flow rate

230 °C

2.6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 2.6 g/10min

dry

ISO 1133

Melt volume-flow rate

230 °C

2.3000000000000003 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 2.3000000000000003 cm³/10min

dry

ISO 1133

Technological properties

Property