Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® XS32 (F-X08057)

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Coefficient of friction, kinetic

0.8 [-]

Show Supplier Material materials with Coefficient of friction, kinetic of 0.8 [-]

dry

ISO 8295

Coefficient of friction, static

1.4 [-]

Show Supplier Material materials with Coefficient of friction, static of 1.4 [-]

dry

ISO 8295

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

dry

Sim. to ISO 62

Water absorption

9.5 %

Show Supplier Material materials with Water absorption of 9.5 %

dry

Sim. to ISO 62

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.47 GPa

Show Supplier Material materials with Elastic modulus of 0.47 GPa

dry

DSM-Method, 50 mm/min

Elongation

350 %

Show Supplier Material materials with Elongation of 350 %

dry

ISO 527-3

Parallel

Tensile strength

96 MPa

Show Supplier Material materials with Tensile strength of 96 MPa

dry

ISO 527-3

Parallel

Yield strength

34 MPa

Show Supplier Material materials with Yield strength of 34 MPa

dry

ISO 527-3

Parallel

Thermal

PropertyValueConditionTesting StandardComment

Coefficient of thermal expansion

9e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K

dry

ISO 11359-1/-2

Parallel

9e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K

dry

ISO 11359-1/-2

Normal

Melting point

218 °C

Show Supplier Material materials with Melting point of 218 °C

dry

ISO 11357-1/-3

10°C/min

Specific heat capacity

1550 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 1550 J/(kg·K)

dry

-

2250 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 2250 J/(kg·K)

dry

Optical

PropertyValueConditionTesting Standard

Transparency

85

dry

DSM method

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt viscosity

260 °C

1120 Pa·s

Show Supplier Material materials with Melt viscosity of 1120 Pa·s

dry

DSM method, 260 °C

Viscosity number

210 cm³/gr

Show Supplier Material materials with Viscosity number of 210 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties