PropertyValueConditionTesting Standard

Density

1.38 g/cm³

Show Supplier Material materials with Density of 1.38 g/cm³

dry

ISO 1183

Moisture absorption

1 %

Show Supplier Material materials with Moisture absorption of 1 %

dry

Sim. to ISO 62

Thermal

PropertyValueConditionTesting StandardComment

Glass transition temperature

80 °C

Show Supplier Material materials with Glass transition temperature of 80 °C

dry

ISO 11357-1/-2

10°C/min

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties

Property
Fillers

50 % Carbon Fiber