General

PropertyTemperatureValueComment

Density

23.0 °C

1.37 g/cm³

Show Supplier Material materials with Density of 1.37 g/cm³

ISO 1183

Moisture absorption

23.0 °C

1.4 %

Show Supplier Material materials with Moisture absorption of 1.4 %

Sim. to ISO 62

Thermal

PropertyValueComment

Glass transition temperature

145 °C

Show Supplier Material materials with Glass transition temperature of 145 °C

ASTM D5026/D7028, from DMTA (tan d)

Melting point

320 °C

Show Supplier Material materials with Melting point of 320 °C

ISO 11357-1/-3, (10°C/min)

Technological properties

Property
Fillers

50 % Carbon Fiber