Arnitel® is a family of high-performance copolyester-based thermoplastic elastomers (TPC) offering a unique combination of flexibility, chemical resistance and high-temperature performance.
Its unique chemistry consists of hard and soft segments which offer a great degree of design flexibility. This includes proven performance in breathable monolithic films, kink-resistant tubing, soft touch applications, and a variety of other innovative solutions for the medical industry.
Because of DSM’s global commitment to manufacturing quality, medical industry leaders trust Arnitel® when material quality and purity is essential for demanding high-precision components.

Datasheet URL:

Arnitel® Care L155E

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

dry

ISO 1183

Moisture absorption

0.2 %

Show Supplier Material materials with Moisture absorption of 0.2 %

dry

Sim. to ISO 62

Water absorption

0.65 %

Show Supplier Material materials with Water absorption of 0.65 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.17 GPa

Show Supplier Material materials with Elastic modulus of 0.17 GPa

dry

ISO 527-1/-2

Elongation

300 %

Show Supplier Material materials with Elongation of 300 %

dry

ISO 527-1/-2

420 %

Show Supplier Material materials with Elongation of 420 %

dry

ISO 527-1/-2

820 %

Show Supplier Material materials with Elongation of 820 %

dry

ISO 527-1/-2

Elongation at yield

20 %

Show Supplier Material materials with Elongation at yield of 20 %

dry

ISO 527-1/-2

Flexural modulus

0.18 GPa

Show Supplier Material materials with Flexural modulus of 0.18 GPa

dry

ISO 178

Hardness, Shore D

52 [-]

Show Supplier Material materials with Hardness, Shore D of 52 [-]

dry

ISO 868

3s

Impact strength, Charpy notched

-30 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m²

dry

ISO 179/1eA

Tear strength

125 kN/m

Show Supplier Material materials with Tear strength of 125 kN/m

dry

ISO 34-1; Method B

134 kN/m

Show Supplier Material materials with Tear strength of 134 kN/m

dry

ISO 34-1; Method B

Tensile strength

41 MPa

Show Supplier Material materials with Tensile strength of 41 MPa

dry

ISO 527-1/-2

Normal

Thermal

PropertyValueConditionTesting StandardThicknessComment

Coefficient of thermal expansion

1.5e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K

dry

ISO 11359-1/-2

Parallel

1.5e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K

dry

ISO 11359-1/-2

Normal

Flammability

HB

dry

IEC 60695-11-10

1.5 mm

UL recognition :Yes

Melting point

207 °C

Show Supplier Material materials with Melting point of 207 °C

dry

ISO 11357-1/-3

10°C/min

Relative temperature index, electrical

50 °C

Show Supplier Material materials with Relative temperature index, electrical of 50 °C

dry

UL746B

2 mm

Relative temperature index, mechanical impact

50 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C

dry

UL746B

2 mm

Relative temperature index, mechanical strength

50 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C

dry

UL746B

2 mm

Vicat softening temperature

90 °C

Show Supplier Material materials with Vicat softening temperature of 90 °C

dry

ISO 306

50°C/h 50N

Electrical

PropertyValueConditionTesting StandardComment

Dielectric constant

4 [-]

Show Supplier Material materials with Dielectric constant of 4 [-]

dry

IEC 62631-2-1

1MHz

4.4 [-]

Show Supplier Material materials with Dielectric constant of 4.4 [-]

dry

IEC 62631-2-1

100Hz

Dielectric strength

21 kV/mm

Show Supplier Material materials with Dielectric strength of 21 kV/mm

dry

IEC 60243-1

Dissipation factor

400 [-]

Show Supplier Material materials with Dissipation factor of 400 [-]

dry

IEC 62631-2-1

1MHz

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt volume-flow rate

230 °C

9 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min

dry

ISO 1133

Technological properties

Property
Application areas

Medical Tubes, Respiratory Tubes