General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | dry | ISO 1183 |
Water absorption | 33 % Show Supplier Material materials with Water absorption of 33 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.12 GPa Show Supplier Material materials with Elastic modulus of 0.12 GPa | dry | ISO 527-1/-2 | |
Elongation | 150 % Show Supplier Material materials with Elongation of 150 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 56.0 [-] Show Supplier Material materials with Hardness, Shore D of 56.0 [-] | dry | ISO 868 | 3s |
Tensile strength | 25 MPa Show Supplier Material materials with Tensile strength of 25 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 185 °C Show Supplier Material materials with Melting point of 185 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 4 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 4 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing membranes, Breathable Outdoor clothing, Smokable Sausage Casings | |
Certifications | Food Contact |