Akulon® K224-HG2

Alternative and trade names
PA6-GF10
Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K224-HG2

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.21 g/cm³

Show Supplier Material materials with Density of 1.21 g/cm³

ISO 1183

Moisture absorption

23.0 °C

2.3 %

Show Supplier Material materials with Moisture absorption of 2.3 %

Sim. to ISO 62

Water absorption

23.0 °C

7.7 %

Show Supplier Material materials with Water absorption of 7.7 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

4.5 GPa

Show Supplier Material materials with Elastic modulus of 4.5 GPa

ISO 527-1/-2

Elongation

23.0 °C

4 %

Show Supplier Material materials with Elongation of 4 %

ISO 527-1/-2

Flexural modulus

23.0 °C

4.2 GPa

Show Supplier Material materials with Flexural modulus of 4.2 GPa

ISO 178

Flexural yield strength

23.0 °C

150 MPa

Show Supplier Material materials with Flexural yield strength of 150 MPa

ISO 178

Impact strength, Charpy notched

-30.0 °C

3 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m²

ISO 179/1eA

23.0 °C

3.8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 3.8 kJ/m²

ISO 179/1eA

Tensile strength

23.0 °C

100 MPa

Show Supplier Material materials with Tensile strength of 100 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

3.5E-7 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.5E-7 1/K

ISO 11359-1/-2, Parallel

Coefficient of thermal expansion, transverse

23.0 °C

1.2E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.2E-6 1/K

ISO 11359-1/-2, Normal

Heat deflection temperature

195 - 210 °C

Show Supplier Material materials with Heat deflection temperature of 195 - 210 °C

Heat deflection temperature, 0.45 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 210 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

195 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 195 °C

ISO 75-1/-2

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ISO 11357-1/-3, (10°C/min)

Relative temperature index, electrical

140 °C

Show Supplier Material materials with Relative temperature index, electrical of 140 °C

UL746B, 0.71 mm

Relative temperature index, mechanical impact

120 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C

UL746B, 0.71 mm

Relative temperature index, mechanical strength

140 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C

UL746B, 0.71 mm

Flammability

<p>HB: 1.5 mm nom. thickn., 1.5 mm, UL recognition: Yes, IEC 60695-11-10</p>

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

ISO 294-4, Parallel

Shrinkage, transverse

23.0 °C

1.3 %

Show Supplier Material materials with Shrinkage, transverse of 1.3 %

ISO 294-4, Normal

Technological properties

Property
Certifications

Yellow Card Available

Fillers

10% Glass Fiber