General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.37 g/cm³ Show Supplier Material materials with Density of 1.37 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.16 % Show Supplier Material materials with Moisture absorption of 0.16 % | dry | Sim. to ISO 62 |
Water absorption | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Glass Fiber |