General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.18 g/cm³ Show Supplier Material materials with Density of 1.18 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.09 GPa Show Supplier Material materials with Elastic modulus of 0.09 GPa | dry | ISO 527-1/-2 | |
Elongation | 275 % Show Supplier Material materials with Elongation of 275 % | dry | ISO 527-1/-2 | |
330 % Show Supplier Material materials with Elongation of 330 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.08 GPa Show Supplier Material materials with Flexural modulus of 0.08 GPa | dry | ISO 178 | |
Hardness, Shore D | 38 [-] Show Supplier Material materials with Hardness, Shore D of 38 [-] | dry | ISO 868 | 3s |
Tear strength | 97 kN/m Show Supplier Material materials with Tear strength of 97 kN/m | dry | ISO 34-1; Method B | |
105 kN/m Show Supplier Material materials with Tear strength of 105 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 13 MPa Show Supplier Material materials with Tensile strength of 13 MPa | dry | ISO 527-1/-2 | Normal |
14.0 MPa Show Supplier Material materials with Tensile strength of 14.0 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 23 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 23 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.75 % Show Supplier Material materials with Shrinkage of 1.75 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Body Plugs |