General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.17 GPa Show Supplier Material materials with Elastic modulus of 0.17 GPa | dry | ISO 527-1/-2 | |
Elongation | 165 % Show Supplier Material materials with Elongation of 165 % | dry | ISO 527-1/-2 | |
320 % Show Supplier Material materials with Elongation of 320 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.16 GPa Show Supplier Material materials with Flexural modulus of 0.16 GPa | dry | ISO 178 | |
Hardness, Shore D | 44 [-] Show Supplier Material materials with Hardness, Shore D of 44 [-] | dry | ISO 868 | 3s |
Tear strength | 74 kN/m Show Supplier Material materials with Tear strength of 74 kN/m | dry | ISO 34-1; Method B | |
75 kN/m Show Supplier Material materials with Tear strength of 75 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 15 MPa Show Supplier Material materials with Tensile strength of 15 MPa | dry | ISO 527-1/-2 | |
16 MPa Show Supplier Material materials with Tensile strength of 16 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 217 °C Show Supplier Material materials with Melting point of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 12.5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 12.5 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property |
---|