General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 6 GPa Show Supplier Material materials with Elastic modulus of 6 GPa | conditioned | ISO 527-1/-2 | |
8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.1 GPa Show Supplier Material materials with Elastic modulus of 2.1 GPa | dry | ISO 527-1/-2 | |
160 °C | 1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | dry | ISO 527-1/-2 | |
180 °C | 1.4 GPa Show Supplier Material materials with Elastic modulus of 1.4 GPa | dry | ISO 527-1/-2 | |
200 °C | 1 GPa Show Supplier Material materials with Elastic modulus of 1 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
3.6 % Show Supplier Material materials with Elongation of 3.6 % | conditioned | ISO 527-1/-2 | ||
120 °C | 4 % Show Supplier Material materials with Elongation of 4 % | dry | ISO 527-1/-2 | |
160 °C | 20 % Show Supplier Material materials with Elongation of 20 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
200 °C | 30 % Show Supplier Material materials with Elongation of 30 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.3 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | conditioned | ISO 527-1/-2 | |
95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 | ||
120 °C | 25 MPa Show Supplier Material materials with Tensile strength of 25 MPa | dry | ISO 527-1/-2 | |
160 °C | 20 MPa Show Supplier Material materials with Tensile strength of 20 MPa | dry | ISO 527-1/-2 | |
180 °C | 15 MPa Show Supplier Material materials with Tensile strength of 15 MPa | dry | ISO 527-1/-2 | |
200 °C | 12 MPa Show Supplier Material materials with Tensile strength of 12 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |
225 °C Show Supplier Material materials with Heat deflection temperature of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber and Mineral Powder |