General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.54 g/cm³ Show Supplier Material materials with Density of 1.54 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7 GPa Show Supplier Material materials with Elastic modulus of 7 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.75 mm |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 3.1 [-] Show Supplier Material materials with Dielectric constant of 3.1 [-] | dry | IEC 62631-2-1 | 100Hz |
3.2 [-] Show Supplier Material materials with Dielectric constant of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz | |
Dissipation factor | 10 [-] Show Supplier Material materials with Dissipation factor of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
130 [-] Show Supplier Material materials with Dissipation factor of 130 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |