General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.49 g/cm³ Show Supplier Material materials with Density of 1.49 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | conditioned | ISO 527-1/-2 | |
13.6 GPa Show Supplier Material materials with Elastic modulus of 13.6 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongation of 5 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 9 GPa Show Supplier Material materials with Flexural modulus of 9 GPa | conditioned | ISO 178 | |
13.6 GPa Show Supplier Material materials with Flexural modulus of 13.6 GPa | dry | ISO 178 | ||
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |
355 MPa Show Supplier Material materials with Flexural yield strength of 355 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | dry | ISO 179/1eA |
23 °C | 27 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 27 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 110 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m² | dry | ISO 179/1eU |
23 °C | 120 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 120 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | conditioned | ISO 527-1/-2 | |
220 MPa Show Supplier Material materials with Tensile strength of 220 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 209 °C Show Supplier Material materials with Heat deflection temperature of 209 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 400 V Show Supplier Material materials with Comparative tracking index of 400 V | dry | IEC 60112 | |
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
5 [-] Show Supplier Material materials with Dielectric constant of 5 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 27 kV/mm Show Supplier Material materials with Dielectric strength of 27 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 240 [-] Show Supplier Material materials with Dissipation factor of 240 [-] | dry | IEC 62631-2-1 | 1MHz |
280 [-] Show Supplier Material materials with Dissipation factor of 280 [-] | dry | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 3e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 2e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 250 °C | 4 g/10min Show Supplier Material materials with Melt mass-flow rate of 4 g/10min | dry | ISO 1133 | |
Melt volume-flow rate | 250 °C | 3 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 3 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | dry | ISO 294-4 | Parallel | |
0.8 % Show Supplier Material materials with Shrinkage of 0.8 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 45% Glass Fiber |