General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Water absorption | 5.4 % Show Supplier Material materials with Water absorption of 5.4 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 8.5 GPa Show Supplier Material materials with Elastic modulus of 8.5 GPa | conditioned | ISO 527-1/-2 | |
12.5 GPa Show Supplier Material materials with Elastic modulus of 12.5 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Elongation of 6 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 11.3 GPa Show Supplier Material materials with Flexural modulus of 11.3 GPa | dry | ISO 178 | |
Flexural yield strength | 275 MPa Show Supplier Material materials with Flexural yield strength of 275 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 24 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 135 MPa Show Supplier Material materials with Tensile strength of 135 MPa | conditioned | ISO 527-1/-2 | |
195 MPa Show Supplier Material materials with Tensile strength of 195 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Thermal diffusivity | 1.09e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.09e-07 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 500 V Show Supplier Material materials with Comparative tracking index of 500 V | dry | IEC 60112 | |
Dielectric constant | 3.3 [-] Show Supplier Material materials with Dielectric constant of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.3 [-] Show Supplier Material materials with Dielectric constant of 4.3 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dissipation factor | 50 [-] Show Supplier Material materials with Dissipation factor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Dissipation factor of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1240 g/cm³ Show Supplier Material materials with Density of melt of 1240 g/cm³ | dry | - | |
Shrinkage | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | dry | ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Shrinkage of 0.9 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2060 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2060 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.28 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.28 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Pedals and Pedal Boxes, Front End Modules | |
Fillers | 40% Glass Fiber |