General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.67 g/cm³ Show Supplier Material materials with Density of 1.67 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 18.5 GPa Show Supplier Material materials with Elastic modulus of 18.5 GPa | dry | ISO 527-1/-2 | |
19 GPa Show Supplier Material materials with Elastic modulus of 19 GPa | conditioned | ISO 527-1/-2 | ||
Elongation | 2 % Show Supplier Material materials with Elongation of 2 % | conditioned | ISO 527-1/-2 | |
2.3 % Show Supplier Material materials with Elongation of 2.3 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 17 GPa Show Supplier Material materials with Flexural modulus of 17 GPa | dry | ISO 178 | |
18 GPa Show Supplier Material materials with Flexural modulus of 18 GPa | conditioned | ISO 178 | ||
Flexural yield strength | 310 MPa Show Supplier Material materials with Flexural yield strength of 310 MPa | conditioned | ISO 178 | |
350 MPa Show Supplier Material materials with Flexural yield strength of 350 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | conditioned | ISO 179/1eA |
23 °C | 13.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13.5 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m² | conditioned | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 210 MPa Show Supplier Material materials with Tensile strength of 210 MPa | conditioned | ISO 527-1/-2 | |
230 MPa Show Supplier Material materials with Tensile strength of 230 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
4.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Glass transition temperature | 120 °C Show Supplier Material materials with Glass transition temperature of 120 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Heat deflection temperature | 250 °C Show Supplier Material materials with Heat deflection temperature of 250 °C | dry | ISO 75-1/-2 | 2 MPa | |
Melting point | 315 °C Show Supplier Material materials with Melting point of 315 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dielectric strength | 30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Notebook Housings, Medium Voltage Circuit Breakers, Medium Voltage Circuit Breakers Embedded Pole | |
Certifications | Yellow Card Available | |
Fillers | Glass Fiber |