General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.42 g/cm³ Show Supplier Material materials with Density of 1.42 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Water absorption | 0.4 % Show Supplier Material materials with Water absorption of 0.4 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 2.3 GPa Show Supplier Material materials with Elastic modulus of 2.3 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA |
Thermal
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 3.2 [-] Show Supplier Material materials with Dielectric constant of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.4 [-] Show Supplier Material materials with Dielectric constant of 3.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dissipation factor | 30 [-] Show Supplier Material materials with Dissipation factor of 30 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Dissipation factor of 200 [-] | dry | IEC 62631-2-1 | 1MHz |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 260 °C | 8 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|