Aqueous Dispersion of Graphene Oxide Powder (GR506040)

.XLSX
.PDF
Save

Properties

General

Concentration c

4 mg/ml

Dispersability

Polar solvents

Monolayer content cmono

95 % at 20 °C

measured at 0.5mg/ml

pH Value pH

2.2 - 2.5 [-]

Chemical properties

Element

Weight %

Comment

C

49 - 56 %

O

41 - 50 %

S

2 - 4 %

H

0 - 1 %

N

0 - 1 %

Technological properties

Color

Yellow-brown

This material data has been provided by Goodfellow.