Tungsten Sulfide WS₂ 99.8% Purity (W556011)

.XLSX
.PDF
Save

Description

Tungsten Sulfide Powder is a dry/solid lubricant powder. It adopts a layered structure related to MoS₂, with W atoms situated in trigonal prismatic coordination sphere.

Properties

General

Density ρ

7.5 g/cm³ at 20 °C

Thermal

Melting point Tm

1250 °C

Technological properties

Application areas

It is used in solutions and semiconductor thin films with applications in optics, electronics, transistors, and energy storage applications. Combined with other materials can be used as catalyst for hydro treating of crude oil.

Other

Particle size: 0.6-10µm

This material data has been provided by Goodfellow.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.