Tribotecc® SLS White fine

Want to keep this datasheet? Save it now in your required format

Description

Solid lubricant based on zinc sulfide and phosphates

This material data has been provided by Tribotecc.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.9 g/cm³

Show Supplier Material materials with Density of 2.9 g/cm³

Particle size D50

10 μm

Show Supplier Material materials with Particle size D50 of 10 μm

Particle size D90

24 μm

Show Supplier Material materials with Particle size D90 of 24 μm

Thermal

PropertyValue

Max service temperature

520.0 °C

Show Supplier Material materials with Max service temperature of 520.0 °C

Technological properties

Property
Application areas

Lubricating greases; lubricating pastes; lubricating coating; plastics

Certifications

NSF Registration No. 152075 (Category Code: HX-1) “Acceptable for lubricant with incidental food contact”

Color

White