Description

The key benefits of Tribotecc® GWZ 300 are: Fully synthetic, temperature stable, improves friction stability at high loads, sulfur carrier

This material data has been provided by Tribotecc.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

4.0 g/cm³

Show Supplier Material materials with Density of 4.0 g/cm³

Particle size D50

0.5 μm

Show Supplier Material materials with Particle size D50 of 0.5 μm

Particle size D90

1 μm

Show Supplier Material materials with Particle size D90 of 1 μm

Thermal

PropertyValue

Max service temperature

520.0 °C

Show Supplier Material materials with Max service temperature of 520.0 °C

Chemical properties

PropertyValue

Zinc

65.8 %

Show Supplier Material materials with Zinc of 65.8 %

Technological properties

Property
Application areas

Friction: Disc brake pads, clutch facings, industrial friction materials, to improve friction stability at high loads; Lubricants: Greases, pastes and oils to reduce coefficient of friction and wear and improve emergency running properties; approved for food grade greases; Plastics: Highly engineered thermoplastics to improve wear and durability; Powder metallurgy: Reduces wear in sintered parts; Other applications: Coatings, powder metallurgy, metal forming

Certifications

Listed in white book - NSF (Registration No. 151012, Category Code: HX-1)

Color

White