Tribotecc® Fibratecc® SF 100 Functional Fibers, Steel Fibers

Want to keep this datasheet? Save it now in your required format

Description

Tribotecc® Fibratecc® SF 100 is a solid lubricant based on functional steel fibers and tin sulfide. The key benefits of Tribotecc® Fibratecc® SF 100 are:

  • A significant decrease of friction resistance by functional fibers that are coated with metal sulfides
  • Therefore less powder solid lubricant is needed
  • Excellent tribological characteristics: The fibers form contact plateaus at those points where friction occurs. Because the fibers are coated with a lubricating layer of metal sulfides, they are wear-resistant
  • A strong reduction of dust, especially respirable particles
  • The non-use of Cu- and Sb
  • Forms protective layers of different contact surfaces over a wide temperature and pressure range


    Fiber InformationLength (mm)Diameter (mm)
    Average20.03
    Minimum0.70.03
    Maximum40.08

  • This material data has been provided by Tribotecc.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    6.3 g/cm³

    Show Supplier Material materials with Density of 6.3 g/cm³

    Sieve residue 45μm

    87 %

    Show Supplier Material materials with Sieve residue 45μm of 87 %

    max.

    Volatile share

    0.1 %

    Show Supplier Material materials with Volatile share of 0.1 %

    at 105°C

    Chemical properties

    PropertyValue

    Sulfur

    15 %

    Show Supplier Material materials with Sulfur of 15 %

    Tin

    7 %

    Show Supplier Material materials with Tin of 7 %

    Technological properties

    Property
    Application areas

    Tribotecc® Fibratecc® SF 100 is characterized by its functional steel fibers and excellent tribological characteristics.

    Combined with the ability to decrease the friction coefficient significantly as well as safe and economical use this product is ideal for a wide range of applications:

    E.g. as a high performance additive for steel industry.

    Color