Tribotecc® MNS 2 Manganese Sulfide (98.5% purity)

Want to keep this datasheet? Save it now in your required format

Description

The key benefits of Tribotecc® MNS 2 are: Fully synthetic, high thermal stability

This material data has been provided by Tribotecc.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

4.1 g/cm³

Show Supplier Material materials with Density of 4.1 g/cm³

Particle size D50

6 μm

Show Supplier Material materials with Particle size D50 of 6 μm

Particle size D90

12 μm

Show Supplier Material materials with Particle size D90 of 12 μm

Thermal

PropertyValue

Max service temperature

400.0 °C

Show Supplier Material materials with Max service temperature of 400.0 °C

Chemical properties

PropertyValue

Manganese

62.5 %

Show Supplier Material materials with Manganese of 62.5 %

Technological properties

Property
Application areas

Friction: Disc brake pads, clutch facings, sintered friction materials, to improve pad and disc wear; Powder metallurgy: Reduces wear in sintered parts, improved machinability, prolongs tool life, chipping aid; Other applications: Diamond/CBN tools, coatings, metal forming

Color

Dark grey

Other

Recommended concentration: 0.2 - 10 %