Description

High strength Mg-free sustainable tube alloys


Use the URL below for more information:

Gränges products

Equivalent Materials

This material data has been provided by Gränges.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

<p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p>

Mechanical

PropertyTemperatureValueComment

Elongation A50

23.0 °C

10 %

Show Supplier Material materials with Elongation A50 of 10 %

Min.

Tensile strength

23.0 °C

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa

Yield strength Rp0.2

23.0 °C

160 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 160 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.36E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K

for 20-100°C

Melting point

611 °C

Show Supplier Material materials with Melting point of 611 °C

Mean

Specific heat capacity

23.0 °C

889 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 889 J/(kg·K)

Thermal conductivity

23.0 °C

160 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 160 W/(m·K)

After brazing, calculated from electric resistivity data measured at room temperature

Electrical

PropertyTemperatureValueComment

Corrosion potential

23.0 °C

-690 mV

Show Supplier Material materials with Corrosion potential of -690 mV

Electrical resistivity

23.0 °C

3.4E-8 - 4.3E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.4E-8 - 4.3E-8 Ω·m

Changes depending on temper

Chemical properties

PropertyValue

Zinc

0.05 %

Show Supplier Material materials with Zinc of 0.05 %

Technological properties

Property
Application areas

Automotive, Heat Exchangers

Corrosion properties

Improved corossion resistance

Processing history

Temper: H24