General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Density of 2.66 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 95 GPa Show Supplier Material materials with Elastic modulus of 95 GPa |
Elongation A50 | 23.0 °C | 0.4 % Show Supplier Material materials with Elongation A50 of 0.4 % |
Hardness, Vickers, 30 | 23.0 °C | 190 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 190 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.67E-5 - 1.77E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.67E-5 - 1.77E-5 1/K | for 20-100°C |
Melting point | 507.1 °C Show Supplier Material materials with Melting point of 507.1 °C | ||
Specific heat capacity | 23.0 °C | 880 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 880 J/(kg·K) | |
Thermal conductivity | 30.0 °C | 135.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 135.5 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.44E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.44E+7 S/m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Powertrain Applications, Cylinder Liners, Automotive | |
Processing history | Spray Compaction, Extrusion, T6 Heat Treatment |