Superior strength, heat treatable material
Dimensions
Standard process capabilities:
Width: 10-1400mm
Thickness 0.050-3.18mm
Coefficient of thermal expansion
α2.36E-5 1/K at 20 °C
for 20-100°C
Melting point
Tm610 °C
Mean
Specific heat capacity
cp889 J/(kg·K) at 20 °C
Thermal conductivity
λ160 W/(m·K) at 20 °C
After brazing, calculated from electric resistivity data measured at room temperature
Corrosion potential
ECP-695 mV at 20 °C
Electrical resistivity
ρel3.4E-8 - 4.3E-8 Ω·m at 20 °C
Changes depending on temper
Element
Weight %
Comment
0.1 %
Application areas
Automotive, Heat Exchangers
Corrosion properties
Improved corossion resistance
Processing history
Temper: H24
This material data has been provided by Gränges.