High Performance Spray Formed Aluminium Alloy DISPAL S270 T4

Alternative and trade names
AlSi25Fe4Ni3CuMgMnCrTi
Want to keep this datasheet? Save it now in your required format

Description

Spray formed aluminium alloy with highest strength and stiffness at high temperature.


Available in Round bars, Flat plates, Customer specifications.


Use the URL below for more information:

DISPAL Alloys

This material data has been provided by Gränges.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.79 g/cm³

Show Supplier Material materials with Density of 2.79 g/cm³

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.52E-5 - 1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.52E-5 - 1.62E-5 1/K

for 20-100°C

Melting point

539.3 °C

Show Supplier Material materials with Melting point of 539.3 °C

Specific heat capacity

23.0 °C

820 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 820 J/(kg·K)

Thermal conductivity

30.0 °C

95.5 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 95.5 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

1.01E+7 S/m

Show Supplier Material materials with Electrical conductivity of 1.01E+7 S/m

Chemical properties

PropertyValue

Aluminium

Balance

Chromium

1 %

Show Supplier Material materials with Chromium of 1 %

Copper

1 %

Show Supplier Material materials with Copper of 1 %

Iron

4 %

Show Supplier Material materials with Iron of 4 %

Magnesium

1 %

Show Supplier Material materials with Magnesium of 1 %

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Nickel

3 %

Show Supplier Material materials with Nickel of 3 %

Silicon

25 %

Show Supplier Material materials with Silicon of 25 %

Titanium

1 %

Show Supplier Material materials with Titanium of 1 %

Technological properties

Property
Application areas

High Temperature-High Strength Industrial and Automotive

Processing history

Spray Compaction, Extrusion, T4 Heat Treatment